TEST
|
REFERENCE
|
REQUIREMENTS
|
CORE-FILL
500™
|
Thermal Resistivity
|
D.O.E. (e)(2)H.U.D.
6.2.7
|
R-Value
not less than 4.0 per inch
|
R
- 4.91
per inch
|
Fire Safety
|
ASTM E-84
|
Flame spread
not to exceed 25
|
Flame
spread* 0
Smoke density 5
|
Corrosiveness
|
D.O.E. (e)(3)H.U.D.
6.2.8
|
Al, Cu, Steel
- no Perforations; Galvanized steel - no pitting; Loss in mass
not to exceed 0.2g
|
No
perforations
No pitting
Less than 0.1g
|
Density
|
D.O.E. (e)(4)H.U.D.
6.1.4
|
Dry 0.7 to
0.9 lb/ft3
Wet 2.5 to 5.5 lb/ft3
|
0.8
lb/ft3
2.7 to 3.3 lb/ft3
|
Water Absorption
|
D.O.E. (e)(5)H.U.D.
6.2.9
|
Not to exceed
15%
No absorption in less than 1 hour
|
Floating
test 3%Droplet test - 1 hr.15 min.
|
Acoustic
Properties
|
ASTM E-90
|
STC Rating
50
|
STC
Rating 53
OITC Rating 44
|
Shrinkage
|
D.O.E.
(E)(11)H.U.D. 6.2.5
|
Not
more than 4.0%
|
Less
than 1%
|